Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Hand Layup
»
Polyester resin outside
Polyester resin outside
Post Reply
Like
10
Polyester resin outside
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
panda
panda
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 47,
Visits: 2.1K
Hi all,
I have a few kayaks to build over the coming weeks using glass and polyester resin. I have build before inside but due to moving house since last building, I will be forced to either rent somewhere, or build outside.
The question is, does building using polyester resin outside affect the finished product as some people have told me that the styrene disappears too quickly meaning the cross linking doesn't happen properly? I have also heard that some larger boat manufacturers build outside when they can.
Layup plan is Gelcoat -> 1x 450gsqm CSM (2 in high stress places for added strength) -> 300gsqm woven rovings all polyester resins. This is the standard layup for the kayaks and works well.
Can anyone help clear this up for me?
Panda.
www.pandakayaks.co.uk
Tags
glass
outside
polyester
styrene
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Polyester resin outside
panda
-
12 Years Ago
I often mould outside and find it works just fine. I'd have no issues doing it at all. 1x450g layer...
FLD
-
12 Years Ago
Thanks :) Its a sprint kayak so long and thin. The only parts which come under a lot of stress are...
panda
-
12 Years Ago
1x200g!! OMG that is thin. I've paddled slalom boats which are 1x600g/3mm foam/2x200g and I thought...
FLD
-
12 Years Ago
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search