Got an answer of Matt,

- The Epoxy gelcoats are with a lid, once opend how long can you keep it? 

With the lid on (or better still wrapped in cling film) so that it’s air-tight you should be able to keep the gel for 6 months.



case closed :p



Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
having the same question Smile EC please respond Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Matt Hislop
Matt Hislop
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Awaiting Activation
Posts: 1, Visits: 34


Hey there,

I've just received my order of various items from easy composites, and I've noticed that the clear epoxy gel coat tin doesn't have a screw on lid.  Instead it has a ring pull and a loose fitting plastic cap.  Would I be right in saying that once opened the tin must be used, i.e you can't reseal it and use it later?

This might seem like a daft question but I thought i'd check before I used it.  

Cheers,

Matt
Tags
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search