By Matt Hislop - 4/10/2012 2:03:52 PM



Hey there,

I've just received my order of various items from easy composites, and I've noticed that the clear epoxy gel coat tin doesn't have a screw on lid.  Instead it has a ring pull and a loose fitting plastic cap.  Would I be right in saying that once opened the tin must be used, i.e you can't reseal it and use it later?

This might seem like a daft question but I thought i'd check before I used it.  

Cheers,

Matt
By matthieutje65 - 5/3/2012 10:55:52 PM

Got an answer of Matt,

- The Epoxy gelcoats are with a lid, once opend how long can you keep it? 

With the lid on (or better still wrapped in cling film) so that it’s air-tight you should be able to keep the gel for 6 months.