Yes you can repair in exactly the same way.  In effect a hole is still a weakness in the tube just on one side rather than a more serious crush type damage.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
sporty
sporty
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 4, Visits: 13
hi ,i have a small whole the size of a match head in a no 7 section so one of the bigger sections, how would you suggest to repair ? as the instructions only seem relevant to a broken or crushed section or would you repair the same ? many thanks .......i have the carbon pole repair kit.