Group: Forum Members
Posts: 198,
Visits: 1.4K
|
I have heard this from an experienced guy before, he used to rub some sort of clearcoat with his fingers into the opened up pinholes. Never actually tried it myself, it's good to get some confirmation.
Regarding the alcohol, I assume because it's less volatile than acetone which evaporates too fast. Fred is literally washing the gunk out of the pinholes with the alcohol and compressed air. More aggressive solvents might attack the sanding dust too much, making it swell and get trapped in the pinholes?
|