Autobody paint shops want to charge me an arm and a leg to have parts coated in urethane clear coat. Is using something like GC50 (https://www.easycomposites.co.uk/clearpol-iso-npg-clear-polyester-gelcoat) going to be comparable to urethane clear coats?

For reference, I'm skinning parts with 2x2 carbon fiber and need UV protection (which the GC50 says it can handle).