Hi Guys,

I came across Z-pins and 'tufting' last night as methods of cross-layer reinforcement.  These are used to stop delamination.  Has anyone got any experience of them or know of any others?  Its always good to know about these things.
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
No experience of the , but have just read up on them, would be interesting to know if there could be a specialist sewing machine that could be used to make a 3d fabric, similar to the z pin idea, but more.

Imagine getting all you different layers of fabric stacked up, then run through a sewing machine to bind them all together with carbon, then infusing