Hi,




Been doing polyester and glass products for a while now but new to carbon and infusion, having a few issues which you guys hopefully can help me with.

Following pictures have been taken in different light and angles to shoe the problem, which I can only describe as voids!

Some details:

Mould is epoxy construction gelcoat+putty, infusion stack is 2 layers carbon 200g +2 glass mat 100g + 1 carbon 200g + peel ply +woven mesh + stretch bagging material. Have tried with a layer of clear gelcoat and without, with gelcoat are the voids you can see on the pictures without and leaves gaps between strands of carbon without resin. Vacuum is good, no leaks and all product procedures are followed.

Here are the pictures 




What is going on here in your option?




Thanks




Chris.
Attachments
Photo0315.jpg (283 views, 554.00 KB)
Photo0317.jpg (284 views, 599.00 KB)
Photo0319.jpg (241 views, 698.00 KB)
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
That looks like the fabric is bridging across the corner. It's just a case of being more careful when laying into the mould
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I would say exactly the same as ajb100

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




chrisdomaingue
chrisdomaingue
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 3, Visits: 17
Ok, thanks for the answers, still does not explain why this happening all over the surface of the parts I make, not as big as what you have seen on the pictures but all over the surface. Your answers have made me think that I forgot to mention I use Profinish carbon mat which has binder backing to stop misalignment of fibres, could that be the cause as fibres cannot be shaped or 'pressed' down properly by the vacuum, as they are held in place by binder?




Thanks for your thoughts.




Chris.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yes I've had issues with that before. To be honest, I don't really like the set-weave fabrics these days. Not for making complete parts anyway, I do like them for cutting strips for decorative surface patterns, but when laying up the whole part itself I much prefer to use standard fabrics. It only takes a bit of practice to learn to handle the fabrics in a way that doesn't distort the weave, and they are much more forgiving when it comes to bridging, which destroys a part much more than a slightly pulled weave.
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
I use pro finish extensively and rarely have voids now... I have had them similar to the pics above but it has always been when I havnt got the cloth laid in the mould perfectly which is quite easy to do.

I use spray tack to secure the pro finish layer and spend more time on this layer making sure it's correct over the entire mould before I move to backing layers.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search