Hi Tony,

The strip should have arrived with you straight so it may well have been damaged in transit.  If You PM us or call us with your order number/details we will sort out a replacement for the bent one.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
tonyfixit
tonyfixit
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 1, Visits: 2
I  purchased some carbon strip, 10mm x 0.5mm x 2m recently from EC.  One strip appears to be curved lengthways at the last 500mm by about 7 mm.  Can I straighten this as I need it for a wing spar?

Cheers

Tony
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search