By tonyfixit - 4/9/2014 8:03:44 AM

I  purchased some carbon strip, 10mm x 0.5mm x 2m recently from EC.  One strip appears to be curved lengthways at the last 500mm by about 7 mm.  Can I straighten this as I need it for a wing spar?

Cheers

Tony
By Warren (Staff) - 4/9/2014 1:58:49 PM

Hi Tony,

The strip should have arrived with you straight so it may well have been damaged in transit.  If You PM us or call us with your order number/details we will sort out a replacement for the bent one.