Hi Scottracing

The rear arches are on my list, probably going to do the rear arches pair after I finish the bonnet air in take mould

Have you seen these carbon-fibre-rear-wings-for-caterham by carbon mods.

Update, some pictures of the extended bonnet mould in progress.


Next build a wooden frame around the back of the mould for support.
Compound back the mould finish, and polish polish polish



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Update of the bonnet air scoop

) Added support frame to mould.
) Pulled first product from the mould!




Edited 12 Years Ago by davro
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
And what a Christmas present it is! Great job! 
wozza
wozza
Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)Supreme Being (8.5K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Very nice, great work Smile

Carbon Copies Ltd
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Very nice looking scoop! Particularly like the use of the Spread Tow carbon down the middle.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Brian2fast
Brian2fast
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
That looks great!  Very cool.

How did you cut the strip of spread tow? Just with scissors?

Craig
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Thanks All

Well pleased with the weight reduction of this part, considering I have raised the height of the new part.

Goal was to reduce the weight of this bonnet air scoop to under 1kg.
This new 4 layer carbon fibre part is around 900 grams, minus some trimming + some clear coat Smile
So the new part is over 1kg lighter than the original glass fibre part + it has a go faster stripe !

The spread tow Go faster stripe was cut with easy composites 8-inch-kevlar-scissors





David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Brian2fast
Brian2fast
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
Is the extra height required for the aluminium supercharger plenum by any chance?...........   Smile

Craig
scottracing
scottracing
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
I really like the use of the textreme instead of doing the usual herringbone v. I might have to do that when i get round to making the bonnet for the caterham Smile
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Hi Brain2fast

It's like you can read my mind, saving up for a dry sumped 1500cc Hayabusa ExtremeEngine + TTS supercharger with aluminium plenum Smile



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search