Group: Forum Members
Posts: 468,
Visits: 2.7K
|
I've seen this with a relatively small cell size. I was wondering if anyone has used it as I was curious to see if you can get away without an inner mould ie lay pre-wetted fabric on top of the core and bag it. I'd have thought it was possible with such a small cell size and some care with wetting the cloth would prevent excess resin filling the cells.
|