Generally speaking you do not need a specific release agent when releasing most resins from silicone moulds.

You will find with some resins, especially some faster curing resins, that over 10-15 releases, the mould will begin to deteriate due to drying of the silicone.  This can be prevented with the use of some pure silicone oil on the mould which helps prevent the drying out.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Djekouk
Djekouk
Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)Supreme Being (202 reputation)
Group: Forum Members
Posts: 30, Visits: 987
Hey,
Yesterday made a silicone mold, and cast some chopped carbon cloth and resin mix.
Didnt use any release and they all came out easy. No release issue at all
:-)
Pault
Pault
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 3
I have made a mould from silicon rubber and wish to cast resin based parts in it.
Do I need a release agent for the silicon mould? if yes then what is best
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search