Wich resin is the best to paint brake calipers of a car
Wich resin is the best to paint brake calipers of a car
Post Reply
Like
8
Wich resin is the best to paint brake calipers of a car
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
lebobo
lebobo
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 2,
Visits: 10
Hello,
I'm a newbie in composite project and then I hope someone could be able to help me to choice the good product...
I wish to know wich resin is the best to paint the 4 brake calipers of my car in red...
As you know, for this project we need an high temperature and long life product and I wish to be able to apply it with a simple paintbrush.
I think exopy resin + red pigments should be ok but I need specialist advice to choice the right products...
Maybe someone has another idea (polyurethan resin ?) Any advice will be very appreciated.
FYI, you can saw a lot of commercial products to do that but they are very expensive (ie :
http://www.g2usa.com/product/CBCP.html)
And here is a video that explain my project :
http://www.youtube.com/watch?v=_ge10FoCeiE
Regards,
Bruno
Edited
14 Years Ago by
lebobo
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Wich resin is the best to paint brake calipers of a car
lebobo
-
14 Years Ago
Hi Bruno, To be honest I don't think that there are any resins systems used in composites that...
Paul (Staff)
-
14 Years Ago
I thank you very much for your prompt answer. Best Regards, Bruno
lebobo
-
14 Years Ago
[quote][b]Paul (Staff) (15/03/2012)[/b][hr]Hi Bruno, To be honest I don't think that there are any...
kylle
-
14 Years Ago
Hi Kylle, We don't have anything like 'plastic dip' - that's probably a little too specific to this...
Matt (Staff)
-
14 Years Ago
Hey there, I saw just the product in Halfords at the weekend. I think it's German. Comes in a box....
Rootz
-
14 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search