posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 13
Hullo everyone my name is Kumar Ranjan. I am working with a formula SAE team.
We are planning on making a carbon fiber body for our next car. In this regard I found out some suitable epoxy resin grades namely Bisphenol F and A. But when I visited suppliers website the names of epoxy were different. As on "easycomposites" epoxy resins are named as EL2 IN2.
How do I differentiate what epoxy I actually need?
Tags
Epoxy resin
FormulaSAE
Reply
Like
8
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Hi, welcome to the forum.
You should create a new topic
here
, as it will be easier seen than in the new member section.
Let us know if you want to laminate your part by hand or if you want to use any vacuum process. It may help deciding which resin to use.
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
9
Krokc
Krokc
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 13
Thanx joe.
I considered your advice and posted it in the correct place.
Well I am planning to go for hand layup.
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search