Resin selection for Bamboo fibre based composite structure
Resin selection for Bamboo fibre based composite structure
Post Reply
Like
3
Resin selection for Bamboo fibre based composite structure
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Nearly
Nearly
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 3
Hello
As part of my university course I have been given the task of considering the feasibility of using Bamboo to create a vehicle chassis structure.
To investigate this I am looking to create some mini prototypes for testing.
What I would like some guidance with, is the selection of a resin to provide the optimum absorption and structural integrity for my application.
Any help will be much appreciated.
Regards
Joe Neale
Reply
Like
3
Reply
Warren (Staff)
Warren (Staff)
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
For a project like this, I would recommend our
EL2 Epoxy Laminating Resin
It has a good all round performance as well as it had good wetting out characteristics and is available with 2 hardener speeds.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Resin selection for Bamboo fibre based composite structure
Nearly
-
11 Years Ago
For a project like this, I would recommend our EL2 EpoxyLaminatingResin It has a...
Warren (Staff)
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search