kylle
kylle
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 34,
Visits: 101
I'm planing to make a carbon brake lever.
Q1: Should a two part mould be strong
enough to do this?
Q2:Now I'm seeing a lot of bike part brands using unidirectional carbon layers to do this kind of works. what do you advise? twill or uni?
example of a carbon brake lever:
Reply
Like
4
Reply
kylle
kylle
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 34,
Visits: 101
MJCT (23/02/2012)
Open your mail box.
didn-t get anything!!!
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Brake lever
kylle
-
13 Years Ago
Q2 - Most forces will be along the levers but not only, for that reason, I believe you should use...
MJCT
-
13 Years Ago
Q1-bad choice of words.... (rusty english) I meant if it's reliable enough to make a clean job....
kylle
-
13 Years Ago
I owna pair of Formula R1 myself but my leavers are made ofmagnesium. Some time ago I also...
MJCT
-
13 Years Ago
Other terms that you should account for are "quasi-isotropic", "nesting" and "stacking" ? what do...
kylle
-
13 Years Ago
Open your mail box.
MJCT
-
13 Years Ago
[quote][b]MJCT (23/02/2012)[/b][hr]Open your mail box.[/quote] didn-t get anything!!!
kylle
-
13 Years Ago
I’ve sent you an email to your Hotmail mailbox on February 22. But I’ll send it again.
MJCT
-
13 Years Ago
The mail goes like this (to much troble to translate every thing, but all you folks can use google...
MJCT
-
13 Years Ago
i think u should use kevlar after 4 layers of carbon and i think u should fill it with resin before...
mhdghoul
-
13 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search