I have some older polyester moulds and I'd love to have a go with the EC pre-preg.  I see that this material isn't recomended for hot mouldings.  Why, what happens to it?  Is it a case of 'its OK for a quick try but constant use fooks it' or is it a case of 'just dont'?
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
when bagged and under high temperatures your mould will have some deformation...delamination is also possible at temperatures to high

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search