By FLD - 1/22/2014 2:25:53 PM

Just following on from another post...

I have some older polyester moulds and I'd love to have a go with the EC pre-preg.  I see that this material isn't recomended for hot mouldings.  Why, what happens to it?  Is it a case of 'its OK for a quick try but constant use fooks it' or is it a case of 'just dont'?
By FLD - 1/23/2014 11:23:36 AM

Thanks guys.  I really appreciate the experience input Smile