Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Its all in the pattern/original part.
As long as the pattern has rolled edge, then as long as you place your flange appropriately and dont use too much filleting wax, then the rolled edge will be transferred to the mould and any parts produced from it.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|