hi guys, 

Im trying to make a mold of a metal watch case and bezel. What would be the best method to use for this? Im going to be using the mold to cast a carbon fiber case. 

Will the gel coat and molding putty work or is the watch case too small for this material. 

Any guidance is highly appreciated. I ve checked through the forum and cant really find anything on this particular question

thanks!  
Reply
jennm
jennm
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 10, Visits: 26
matthieutje65 (12/01/2014)
you just repeat the same step on the other side Smile just add some releaseagent on part and mould that will be covered again... but keep in mind you have to watch out for undercuts... if you have some undercut with silicone you can just bend it... when you work with gelcoat and so on it can be much harder


thanks again man, i will give it a go
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
jennm - 12 Years Ago
jennm - 12 Years Ago
TomDesign - 12 Years Ago
jennm - 12 Years Ago
redrumredrum89 - 11 Years Ago
Zero Mass Motorsports - 11 Years Ago
matthieutje65 - 11 Years Ago
jennm - 11 Years Ago
matthieutje65 - 11 Years Ago
jennm - 11 Years Ago
matthieutje65 - 11 Years Ago
jennm - 11 Years Ago
                             Do you have any pictures of your mould?
matthieutje65 - 11 Years Ago
                                 [quote][b]matthieutje65 (10/01/2014)[/b][hr]Do you have any pictures of your mould?[/quote] hey...
jennm - 11 Years Ago
                                     I would rather go for that second option... You need a hard moulding surface so you can build up...
matthieutje65 - 11 Years Ago
                                         [quote][b]matthieutje65 (11/01/2014)[/b][hr]I would rather go for that second option... You need a...
jennm - 11 Years Ago
                                             you just repeat the same step on the other side :) just add some releaseagent on part and mould that...
matthieutje65 - 11 Years Ago
                                                 [quote][b]matthieutje65 (12/01/2014)[/b][hr]you just repeat the same step on the other side :) just...
jennm - 11 Years Ago
Shaneer22 - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search