Beginner making mold, seeking help


Author
Message
susej1981
susej1981
Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)
Group: Forum Members
Posts: 2, Visits: 32
I'm making a wet layup mold so I can replicate my car's doorsills in carbon fiber. door sills in question are plastic BMW E30 sedan ones.

I wanted to check with someone who knows what they're doing whether my mold will work well or not.

 I plan on gluing sheet styrene on top of my birch baseboard, and then on top of the styrene I plan on hot gluing my trim from the bottom. I know I'm going to need to make some fillets around all the sharp edges to avoid mechanical adhesion but can I use MMD green hobby putty instead of plasticine/oil based clay/yellow filleting wax (like I see a lot of people using on the forums)

also, I'm not sure how I plan on making a flange on the triangular piece of the trim. I drew a crude side view in MS paint to help illustrate my ideas but if anyone has a better idea I'd love to hear it.

I wanted to ask, do I need specific pigmented tooling gel coat or can I just mix up some polyester resin and let it get tacky and start laying on my fiberglass matt? I watched the video by carbon mods and he uses a thick lime green gel coat to make a mold of his replica part and I also see a lot of people using this same technique.

thanks a bunch
Edited 12 Years Ago by susej1981
Reply
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Hi, I don't know what you have done with those links. I can't click on them and I can't copy and paste them. Please try again.

Brian.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search