wojtepanik
wojtepanik
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 102,
Visits: 582
Hi!
I use vaccum bagging and I want to kill all the pinholes. I was wondering, can I spray clear coat on mould after puting release agent, after laquer I would put normal layup. Will the clear coat release? Will it bond to polyester or rather epoxy? I've talked to Mathieu and he said that it would be ok put first layer should be thin and after it doesn't matter.
Thanks for taking your time
Wojtek from Poland
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Edited
12 Years Ago by
wojtepanik
Reply
Like
3
Replies
baja_patient
baja_patient
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 135,
Visits: 1.6K
There is something called an IMC (In-Mould Coating), available in clear and many other colours. You spray it directly into the mould and then proceed with normal layup.
HP-Textiles in Germany sells it.
http://www.hp-textiles.com/shop/advanced_search_result.php?keywords=hp-imc-0000&XTCsid=7b9829cd7e1246659e3de7842e10dd3c
cheers
Reply
Like
3
wojtepanik
wojtepanik
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 102,
Visits: 582
baja_patient (13/12/2013)
There is something called an IMC (In-Mould Coating), available in clear and many other colours. You spray it directly into the mould and then proceed with normal layup.
HP-Textiles in Germany sells it.
http://www.hp-textiles.com/shop/advanced_search_result.php?keywords=hp-imc-0000&XTCsid=7b9829cd7e1246659e3de7842e10dd3c
cheers
Hi,
It looks ok for me, I can probably import it on my own but I'll find some similar product here in poland
Thanks
Wojtek from Poland
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Spraying clearcoat directly on mould...
wojtepanik
-
12 Years Ago
It depends which clear coat you use and the prep beforehand. I have heard that Marineware in...
ChrisR
-
12 Years Ago
There is something called an IMC (In-Mould Coating), available in clear and many other colours. You...
baja_patient
-
12 Years Ago
[quote][b]baja_patient (13/12/2013)[/b][hr]There is something called an IMC (In-Mould Coating),...
wojtepanik
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search