Suggestion for 2K clear coat spray can?


Author
Message
StanTheMan
StanTheMan
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 61, Visits: 380
Hi guys,

I recently came across a post by a member here who mentioned 2k clear coat spray but in a can. I searched the web, even youtube and came across some pretty amazing stuff. From what I've seen, there's absolutely no competition between the normal aerosol clear coat spray can and the 2K. Some 2K's even claimed that they had 4 times the pressure of a normal aerosol clears. Not sure how true that is but anyway... I haven't got the funds to afford a proper airgun or an air compressor so I'm looking for cheaper alternatives. I've been working with Dupli-Colour clear spray can and I've gotten very bad results. I can never get a full gloss. EVER. Sometimes I even get a matte finish... Anyway, I just wanted to ask you guys whether the 2K clear coat spray cans are THAT good compared to the conventional one component ones, and maybe you can recommend a brand to me. Bear in mind that I'm not in the UK and it'll be splendid if I could order it online.

Regards,
Stan
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Maybe it is the way you use the spraycans? I use Motip and get good results with it...
Keep in mind that you have to apply multiple soft coats (not one big coat at once) sand it inbetween, add clearcoat again in a few time sand and then polish...
I recently used 2K primer and worked out great! it is much "stronger" than 1K spraycans. I'll upload a video soon on my Youtube-channel about my experience with 
that 2K spraycan

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com