I've always got by using celotex/kingspan foam to make plugs in the past but I'm now preparing o make my biggest plug yet as body work for a vehicle, its about 2m long and 600mm wide.

Even if I made a wooden structure in the middle to minimise the foam usage, its still going to cost a fortune, so I'd been considering trying polystyrene. I know I can't use any styrene based resins, and the surface detail is going to be terrible so it'll need a skim of filler all over, but can you use 2k paint on polystyrene?

What does everyone else use for large plug making? Are there cheaper foams I could be using?
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
wojtepanik (16/11/2013)
Hi!
What exactly kingspan foam you use? Warren, you are making custom lotus 7, is it the same as caterham? 
Bye!
Wojtek from Poland


Hi Wojtek, yes it is similar to a caterham. I have attached a picture of a 1/10th scale model of the design. Kingspan is just a trade name, it is just standard building grade insulation board with the foil coating removed.

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search