Hi I ordered VI Starter kit.

My Vaccum pump is working but It looks little bit out of order

It pulls vaccum until 90% well. but when it comes to 90% and about 5seconds later,  It's noise nevel is much louder. and it can't proceed more than 90%

I hope vaccum gage is not accurate.. but noise sounds out of order. The sealing is perfect (I onlt test with the catch pot and when I turn off the turn valve, there is no leak)





and when I turn off the vaccum pump without turn valve off, the air leaks from the vaccum pump quite fast. is it OK?
carbonfibreworks
carbonfibreworks
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
With the pump running and connected to your catch pot turn your pump valve from the closed to open position, if the noise level increases you have an air leak. Have you filled the pump with oil to the correct level ?
Chris 
www.carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
giganoto
giganoto
Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)
Group: Forum Members
Posts: 2, Visits: 9
even if the turn valve is off(Close), noise level increase. The oil is in proper level

I guess air leak is in the pump.. 
ChrisR
ChrisR
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
unscrew the connector & valve from the pump, clean the threads and put back together with PTFE tape around the threads (plumbers tape) as this will help seal (or elimate this as an issue)