Hi, I am thinking of using some of your tooling gelcoat to make a mould off a part.  Does anyone know what kind of time (min and max) I need to wait between applying the first coat, and applying the second and then applying the layup?  I belive you cannot leave the gelcoat too long between coats as then the next layer will not adhere to it correctly.  Also can this gelcoat be used at 15 or 20 degrees c insted of 25 (I understand cure times will be longer)?

Aother question I have regarding this gelcoat is can it be used as a topcoat, I.E. applied over a layup and then sanded when cured?

Many thanks, lee.
Edited 12 Years Ago by Leew
Reply
Leew
Leew
Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)
Group: Forum Members
Posts: 33, Visits: 187
Due to my work meaning I don't very often get 8 hours all in one go, I was wondering is it possible to put the two layers of gelcoat on the mould, then leave it 24 hours, then sand it to give it a key before laying the reinforcement?  Will it be strong enough to not pull off in chunks when releasing parts from the mould.  I used 6 coats of easylease as a release.