I've basically made a few fruit bowls that  I'd actually like to store fruits in them. My question is, what kind of treatment or topcoat should I put on the bowls. Obviously food and epoxy is a no no. Some kind of a non-toxic clear coat? Thanks in advance
Reply
Leew
Leew
Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)
Group: Forum Members
Posts: 33, Visits: 187
EC fibreglass sell a resin which they say is food safe when post cured to 80c
see http://www.ecfibreglasssupplies.co.uk/p-1504-crystic-491-pa-resin-including-catalyst.aspx