Hi guys,

I am currently in the process of creating some patterns using your High Density Polyurethane Foam. I am planning to take them to a high gloss finish that is reasonably rugged and will withstand several moulds being duplicated off it.

I will take them to a paint shop to have to 2k primer filler applied and get it to a gloss finish as i don't have good enough equipment for 2k paint. Is it possible for the paint shop to get the finish i want just using 2k filler primer?

Secondly how should i prepare the foam for them? Should i coat it in a thin layer of FG tissue and resin or will it be fine bringing it to them showing foam?

I'm just look to sort out any issues before i look around for a good body shop to do the work. As i will need it done relatively quickly once the foam is done.



Thanks,
Dave.
Reply
Dave
Dave
Supreme Being (554 reputation)Supreme Being (554 reputation)Supreme Being (554 reputation)Supreme Being (554 reputation)Supreme Being (554 reputation)Supreme Being (554 reputation)Supreme Being (554 reputation)Supreme Being (554 reputation)Supreme Being (554 reputation)
Group: Forum Members
Posts: 48, Visits: 253
Hi all i was wondering if i could get more details on a method shown on the EC website under a Q&A section 



"If I machine this block to the shape I want, how do I seal it to make mouldings from? and what thickness do I need to add?"

Part of the EC reply "A layer of epoxy resin mixed with glass bubbles (to make it sandable) and some coloidal silica (to make it thick) makes a very good 'pattern coat' which once cured can be sanded and polished up to a gloss."…


is it possible to get more details on this method like ratios of glass bubbles and coloidal silica?

Thanks,
Dave O.


Edited 14 Years Ago by Dave
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search