Hi everyone!

I could use some advice...
So I draw my part in software and those were CNC-milled in multiplex wood.
I know wood isn't the best choice but for me as a student it was the cheapest way...

The finish is good but I'm wondering how I have to finish the moulds before filling them with an epoxy to get the plugs out.
I'll finish those plugs once again till a high gloss then. The wooden moulds will only be used once to get the plugs.
I have some ideas but wondered what your experiences are with those kind of problems.

1. Coat the mould with a Infusion Resin with a brush a few times.
2. Use vinyl wrapping (carwrapping vinyl to seal everything
3. Use a 2K filler spraycan. and sand till high gloss

I would prefer choise 3 but I need to have a confirmation telling me it wont react with epoxy after it... 
I read it a lot its ok to do it that way but just need the confirmation if possible Smile

http://www.talkcomposites.com/Uploads/Images/467cadab-d61c-4e80-b0e1-0c79.JPG

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Ok thanks, The problem is I'm quite limited in material to spray resins, coatings and so on so I thought the best/easiest/cheapest way for me is spraycans, but want to be sure it wont react with the wood and so on...but I'll give it a go I think Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search