Group: Forum Members
Posts: 363,
Visits: 3K
|
Just use acetone, it doesn't leave any residue on the brush, cleans thoroughly and won't dry out in the pot if you put a lid on it.
Clean the brush in the acetone using stippling action etc until clean then dry the brush completely using a clean rag/lint free cloth, put lid on pot. job done, you can reuse the brush as soon as it's completely dry with minimal risk of contamination
|