How to Make an Accurate Composite Pattern (Buck) by Hand


Author
Message
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Here it is then folks, a professional video tutorial from the Easy Composites team, this time on composites pattern making. We'll give you a step-by-step process that can be followed to enable you to reliably produce dimensionally accurate and well finished glossy patterns for any design idea that you have.

We use a new design for a carbon fibre airbox (a product we actually need for our demo car!) and show taking a 3D CAD design, printing out templates from it and making the basic shape from foam before coating it and finishing it. We know that pattern making can be pretty daunting and I really hope this video shows that if you take your time and have a good process to follow it should not be anything to worry about!



As with all our recent videos this is shot (and best appreciated) in full HD which is far more effective at 'putting you in the room' than watching the low res version so please link through to the Pattern Making Video Tutorial page and change your YouTube settings to 1080p to appreciate it at its best.

If you have any questions at all about the process then please post your questions here where myself, Paul or Warren would be very pleased to answer your questions.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 12 Years Ago by Matt (Staff)
Reply
r0bsk1
r0bsk1
Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)
Group: Forum Members
Posts: 38, Visits: 307
I'm making something similar myself. Are you going to do a 'how to' for the finished airbox?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search