Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Kevlar honeycomb.
Kevlar honeycomb.
Post Reply
Like
5
Kevlar honeycomb.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
wojtepanik
wojtepanik
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 102,
Visits: 582
My supplier has something called kevlar honeycomb, as far as I know it is made out of kevlar paper(?) pre-impregnated with phenol resin. It is realyyyy expensive 70euro exl.vat for 2mm x 2550mmx1250mm and 48kg/m^2, he claims that it is the lightest sandwich in the world. I don't have money to buy it, but when I have some $ I will make some reviev of that, this is how it looks like :
Here are some more info but unfortunatly in polish, but I quess it is not hard to understand things like dimensions or price
http://surfpol.pl/materialy-sandwichowe-menukompozyty-112/honeycomb-aramid-menukompozyty-118.html
Do you know anything about it? How strong is it? Is it hard to work with? Is it worth buying?
Thanks for your time
Wojtek from Poland
Bye!
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Edited
12 Years Ago by
wojtepanik
Reply
Like
5
Reply
Florin Andrei
Florin Andrei
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 11
Beginner question: Let's say I make two flat panels. They are the same size, roughly as big as a regular computer monitor.
For panel A, I just make one solid sheet of CF, from 8 layers of CF cloth soaked with epoxy, then vacuum-squeezed until cured.
For panel B, I make a sheet from 4 layers of CF, cure it until solid, epoxy a 5 mm Kevlar honeycomb to it, then make another 4-layer sheet and epoxy that one to the other side of the honeycomb.
What would be the differences between panel A and panel B from a mechanical standpoint? What would be some typical applications where panel A would be desirable, and what would be the cases when I would prefer panel B?
Edited
12 Years Ago by
Florin Andrei
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Kevlar honeycomb.
wojtepanik
-
12 Years Ago
You can see this type of material a lot on different expo's and so on. They use it for aero-projects...
matthieutje65
-
12 Years Ago
As a raw core, it certainly isnt the lightest in kg/m3 Some aluminium honeycombs with a large cell...
Warren (Staff)
-
12 Years Ago
Beginner question: Let's say I make two flat panels. They are the same size, roughly as big as a...
Florin Andrei
-
12 Years Ago
The best way to compare is with like laminate to start with. This image from the FSAE website shows...
Warren (Staff)
-
12 Years Ago
Aren't foam core composites weaker in shear? Let's say the top CF panel moves left, and the bottom...
Florin Andrei
-
12 Years Ago
Hi, I have done a few small testing parts using both Alu-honeycomb (small cell EC stuff) and...
Dravis
-
12 Years Ago
Florin, it all depends on your specific application. Such severe shear loading would probably not be...
Warren (Staff)
-
12 Years Ago
[quote][b]Warren (Staff) (29/10/2013)[/b][hr]This is my test panel using 25mm aluminium honeycomb...
Florin Andrei
-
12 Years Ago
The 1mm skin was a layer of 200gsm 2/2 twill and a layer of 650gsm 2/2 twill resin infused. The 2mm...
Warren (Staff)
-
12 Years Ago
Is that not nomex honeycomb? if not how does it compare to nomex? Just for reference I've built...
Ledon Racing
-
12 Years Ago
Both Nomex and Kevlar are DuPont registered trademarks for slightly different versions of...
Dravis
-
12 Years Ago
wow that panel is certainly impresive! i wonder how in practical terms you might mount something...
benet
-
12 Years Ago
To add fixings to composites you generally need a way to spread the load and prevent "rip through"....
Warren (Staff)
-
12 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search