Hello,

I just received  a new Vacuum Degassing System - Small Vacuum Pump. 
After toping the Oil as per instructions, I am running some trial runs. During these,  I noticed a significant amount of Oil in the vaccum chamber (see image below). 
Otherwise the pump pulls a vacuum. 

Is there a step I am missing which is leading to this issue ?

Many thanks,
Jean P
http://www.talkcomposites.com/Uploads/Images/f0f5543f-4db3-4971-a20c-fea8.jpg
Reply
jeangui
jeangui
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Thanks Warren for the prompt feedbacK.

So if I understand correctly, one needs to close the valve before switching it off. Correct ?
What about when turning it on. Does it matter if the valve is open or closed ?

Thanks again.
Jean
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search