posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 4
I have a customers carbon bike frame which has an issue where the headset, which has an interference fit aluminium cup that presses into the frame, has become loose due to the carbon frame having worn giving about 1 mm of movement in the cup.
I plan to replace the cup with a type that has a removable bearing from the cup, thus allowing me to bond the cup into the frame to eleviate the movement in the headset.
So finally the question!
What I need to know is what product you would recommend to bond an aluminium cup into a carbon fibre frame that would take the knocks that a mountain bike will endure and fill the small voids that now exist between frame and cup?
Many thanks for your help.
Simon.
Reply
Like
3
Reply
wojtepanik
wojtepanik
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 102,
Visits: 582
Hi!
Maybe it is not the way it should be done, but I would do it this way : mix some epoxy resin or glue with graphite or micro-sphere and put chopped cf strands and mix well, after cleaning the surface wedge the mixture between, you may sand all the surface with some heavy grid to have nice bonding surface. Thats my way to do it, I'm not professional but it worked in all my repairs. The strands have to be chopped to really small pieces.
Bye
Wojtek from Poland
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Product Advice
Sy
-
12 Years Ago
I would personally use Araldite 420 for that....
Leew
-
12 Years Ago
Hi! Maybe it is not the way it should be done, but I would do it this way : mix some epoxy resin or...
wojtepanik
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search