Vinylester mould and expanding polyurethane - release?


Author
Message
LaxFriedrichs
LaxFriedrichs
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 58, Visits: 450
I'd like to use expanding polyurethane in part of a vinylester mould  (Unimould system) I have made, to make a plug

The mould surface is a high gloss.

The cured foam plug doesn't have to have a perfect surface, it just has to release -  in one piece!! I have Easylease, and EC mould wax to hand...



Thanks for any help
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
For polyurethane I use a release agent called "APW" spcialy made for Polyurethane... I noticed it didn't work with a release wax... maybe the chemical easylease will work?!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




LaxFriedrichs
LaxFriedrichs
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 58, Visits: 450
Thanks Matthieu.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search