Hi Wojtepanjk,
Other archers of this type of compound bow, have been experimenting with other materials, and one such example is that the limbs have been made from aluminum only. That's not exactly a flexible material, however the bow does work. I'm looking to make the bow as light as possible, the carbon fiber wouldn't be for appearance sake. Also the riser is not required to be flexible, its a rigid component, currently made of aluminum, why couldn't the riser be replaced with a carbon fiber version?
|