can anybody recommend a decent wax or clay to use when making moulds? the colour clay i have is quite think and can break at corners when smoothing with my finger or spreader.


Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi, Jap.

I use this stuff from EC and it works great. I used it with EC epoxy gelcoat (the green one) and mold putty as well with the Unimold process, and was not disappointed.

Its more expensive than regular plasticine, but you can still reuse it reasonably.

Being a wax, the heat of one of your hand holding a small amount while you are working with ur other hand will keep it soft enough to be very workable without applying tons of pressure to shape it.

Hope it helps.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Edited 13 Years Ago by Joe
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search