Cold casting for model engineering, using metal fillers. What would be the best resin for this?

I would like to make castings for flywheels for example, 4 - 6 in diameter.

I tried to cast a 2 inch cube filled with iron powder but it got very hot melting the plastic mould.

Any thoughts?

Alexanm
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
thats a large cube to do in one time? mostly when you want to cast "big" objects you have to do it in small layers (max 1cm at the time)
the exothermal reaction of some resins can build up quit some heat and the more you make at once the faster it will cure and the hotter it will get...
causing some cracks and 'burned' resin...

I mostly use PU casting resin and have already added some graphite powder in it and worked out perfectly

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search