Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
I've just experimented with standard addition cure casting silicone. Seems to work ok. There may be other specialist silicones for the job out there. Just bear in mind it needs to have a service temperature high enough to withstand the curing of the pre-preg.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|