Mostly interested in epoxies yeah, but I would be interested in anything TBH. I'm a chemist so I was looking for a little academic stimulation. It seems like the larger polymer numbered resins have better mechanical properties but then are mega viscous.
A complete swerve ball but do you know if anyone has produced an epoxy thread? It'd be interesting if this could be incorperated into the cloth and crosslinked on lay-up. It'd need some short chain resin to fill in but could work well.
I'm also interested in any alternative new tech. I have vague memories of a thermoplastic thread interwoven that melted on bake. Resin free system! I think Carr made that one.
|