I made a 16mm diameter x 300mm rod from clear epoxy casting resin as a test. It bounces when dropped and is slightly flexible. I also used it for casting some 28mm soldiers which were very strong where as the fast cast PU resin was very brittle. I would rather not say where I got the resin from as it may be unfair to Easy Composites, unless Warren says I can, as they have nothing suitable.