Wondering what people use to align and attach mould sections?

I've seen these http://www.grpmouldclamp.co.uk/

Are they a good option?

Cheers,
James
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Looks like a well engineered solution. 

Nothing wrong with drilling through and using nuts and bolts if you can mould in an interlock.  Half spheres make great way of interlocking your flanges when used during the moulding process.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ajb100
ajb100
Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
I use a big blob of filleting wax on the flanges
compositepro
compositepro
Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)
Group: Forum Members
Posts: 22, Visits: 65
Ledon Racing
Ledon Racing
Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)
Group: Forum Members
Posts: 12, Visits: 74
I make my own half spheres from solid resin that are drilled a tapped from behind or just stuck in place before I lay up the mould. Then I generally use M8 bolts and penny washers to clamp them up.

www.LedonRacing.com

Professional motorsport services
& composite production / repairs.



FLD
FLD
Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I've used impact rivets before as half spheres but for really good locations I use a washer in the plug to leave a round hole and then I use pattern makers dowels.  These are used for mould location when metal casting.

Halfway down here:

http://www.stationroadbaseboards.co.uk/cart_dowels.htm
Ping G
Ping G
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 1, Visits: 10
Hi,  I'm new here and came across this topic.

I use marbles, cheap and easy to come by.  When doing split molds, I use them as locating pins.  Once the plug is done, a parting board is cut to the dimensions required, with the shape of the plug in the middle.  

Marbles are imbedded halfway using body putty, the parting board is installed, waxed, and the side of the plug where the marbles are, is laid up.  

Once the resin has cured, remove the parting board, clean and wax the mold face, lay up the other half.  The shape of the marbles will make alignment perfect every time.  Picture show a marble still imbedded in a parting board with removed marbles beside it.  Other picture shows the locating pins in a mold set.

Ping
Attachments
IMG_0687.JPG (833 views, 2.00 MB)
IMG_0685.JPG (787 views, 1.00 MB)
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Ping G (23/10/2013)
Hi,  I'm new here and came across this topic.

I use marbles, cheap and easy to come by.  When doing split molds, I use them as locating pins.  Once the plug is done, a parting board is cut to the dimensions required, with the shape of the plug in the middle.  

Marbles are imbedded halfway using body putty, the parting board is installed, waxed, and the side of the plug where the marbles are, is laid up.  

Once the resin has cured, remove the parting board, clean and wax the mold face, lay up the other half.  The shape of the marbles will make alignment perfect every time.  Picture show a marble still imbedded in a parting board with removed marbles beside it.  Other picture shows the locating pins in a mold set.

Ping


Exactly Ping! Good thinking, thats how i tackle mine too. No need faffing around with embedded sockets that need to line up in the first place to when building the mould anyway. 

Half spheres, n  then bolt em together. easy as. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search