Some form of shears to cut the fabric. Choose which ever suits you best.
Gloves - you'll use loads.
Maybe Acetone - helps clear up uncured resin.
Perma-grit tools to trim and finish off
Digital scales - if you can't get away with borrowing the kitchen ones!!
Thermometer - you need to accurately know the garage temperature for resin curing purposes. A lot of customer problems are due to inaccurate estimates on temperature.
Old clothes/Apron - cured resin makes a mess of clothes, plus you won't want carbon fibres on your best clothes and dragged through the house!!
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|