I recently made my first mould and found out it might have been a bad idea to use rattle can spray paint with this being the result



I want to know if I clean away all the paint with standard thinners am I also effecting the gel coat? A quick rub with a cloth soaked in thinners didn't appear to rub of any gel coat so it seems harmless enough but I'd like to know if this is true or that it does effect the coating?
Reply
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
honestly if i some time ago got that shape mold i simply trashed it and made nice new straight and glossy as cleaning taking and fixing more time then to make new and not hold so good as new Wink