I use a 3 to 1 Epoxy from Composite Envisions.com
and the layers vary until i have a uniformed flat surface. All of these parts I did as Overlay on the original parts, not Vacuum Form, or Infusion. They are original parts wrapped in carbon fiber and resin up, sanded down and resin up over until i am satisfied. Many tell me that they actually look like vacuumed carbon pieces.
|