I agree with Matthieu on this one. Even with a crease free filmor using a perforated release film instead of peel ply, you're still going to have a lot of work to do.
Rememeber with infusion the resin layer will be quite thin leaving little to sand before you damage the carbon.
Not to forget the practicalities on some car parts with vacuum bagging on the originals.