Silicone bag with EC Addition Cure Silicone Rubber


Author
Message
coliveira
coliveira
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 2, Visits: 13
Hello,

I would like to know if the product  Addition Cure Silicone Rubber will work as a silicon bag.

Regards,
Cristiano

Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Cristiano,

Yes, it definately will. In fact we have many examples here at EC headquarters of silicone bags made using our Addition Cure Silicone Rubber. The one important thing though is that you will need to add some of our Thixotropic Additive for Addition Cure Silicone Rubber - this makes the silicone thicker and so turns it into a 'brushable' silicone. You only need a tiny amount so just buy the 50g pack.

I hope this information helps.

Best regards, Matt


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
coliveira
coliveira
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 2, Visits: 13
Hi Matt,

Thanks a lot. I will buy that.

Regards,
Cristiano
fgayford
fgayford
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hi Matt
Very interesting . Could you show us a few pictures of these bags you are using?
Thanks
Fred
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search