Hello Guys,

Need an opinion from experts here.

Does GC50 Epoxy Compatible Gelcoat goes along well with Vinylester based resin? Anyone have experience with this combination?

regards//Azrul
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Azrul,

I'm not 100% clear from your post whether you want to know if the GC50 would be suitable as a gelcoat for vinylester based parts or whether you want to know whether GC50 would release nicely out of a vinylester based mould so I'll answer both scenarios.

If you were making parts out of a vinylester resin then I would not recommend that you use GC50 as an in-mould gelcoat (before laying up with the vinylester resin). GC50 is designed to be bonded to by epoxy resin and although there is some crossover in the chemistry of vinylesters with epoxy you won't find that a vinylester resin will bond properly to the GC50 Epoxy Compatible Polyester Gelcoat. Instead, it would be better (and cheaper!) to simply use a high quality Clear Polyester Gelcoat.

If instead you'd meant would the GC50 release nicely out of a mould that's been made using a vinylester gelcoat (like our Uni-Mould Tooling Gelcoat) or a vinylester resin system then yes, it would be perfectly fine. A good number of the members on this forum who are using GC50 are probably spraying (or brushing it) into vinylester based moulds.

I hope this helps,

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search