Epoxy resin & thixo additive?


Author
Message
chemie29
chemie29
Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)
Group: Forum Members
Posts: 18, Visits: 75
Hi everybody! I have a question for you. Witg application in moulds with vertical walls, is it necessary to use some thixotropic epoxy resin or can I use a standard one? Thanks
Reply
fiberglasshawaii
fiberglasshawaii
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 7
You could, or you could add some aerosil to your mixture to thicken up the resin you do have. We get a lot of marine/canoe builders that figured out different work arounds so you don't have to buy multiple resins.
http://shop.fiberglasshawaii.com/resin/fillers-97/flas-aerosil

Fiberglass Hawaii Inc.
Oahu - Maui - Ventura

http://shop.fiberglasshawaii.com
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search